Skip to main content

Table 2 The table shows the types of polymer captured from the Natabua WWTP and identified using the ATR-FTIR. The first section of the table shows the percentage (%) of each type of MP from a stage and the next section describes the number of MP per 10L sample

From: Influence of different Wastewater Treatment Processes on the rate and characteristics of MPs released from WWTPs in Fiji, South Pacific

MP—Type of Polymer

Anaerobic

Facultative

Maturation Outlet

Anaerobic MP/10L

Facultative MP/10L

Maturation Outlet MP/10L

Cellophane

23%

10%

33%

0.70

0.10

0.50

Polyester

3%

23%

-

0.10

0.30

-

Polypropylene

-

15%

17%

-

0.20

0.10

Polyvinyl propionate acrylate

-

-

-

-

-

-

Polyethylene

19%

38%

33%

0.60

0.50

0.20

Polyvinyl Acetate Ethylene

-

-

-

-

-

-

Polyester

3%

-

-

0.10

-

-

Polyamide

-

-

-

-

-

-

Polyvinylidene fluoride

-

-

-

-

-

-

Polyethylacrylate

10%

-

17%

0.30

-

0.10

Alkyd Resin

6%

-

-

0.2

-

-

Alkyd Urethane

-

8%

-

-

0.1

-